MG Chemicals 4870-18G Sn60/Pb40 No-Clean Leaded Solder Wire, 0.032" (0.81 mm), 18 g (0.6 oz) Pocket Pack
MG Chemicals 4870-18G Sn60/Pb40 No-Clean Leaded Solder Wire, 0.032" (0.81 mm), 18 g (0.6 oz) Pocket Pack
MG Chemicals 4870-18G Sn60/Pb40 No-Clean Leaded Solder Wire, 0.032" (0.81 mm), 18 g (0.6 oz) Pocket Pack
  • Load image into Gallery viewer, MG Chemicals 4870-18G Sn60/Pb40 No-Clean Leaded Solder Wire, 0.032" (0.81 mm), 18 g (0.6 oz) Pocket Pack
  • Load image into Gallery viewer, MG Chemicals 4870-18G Sn60/Pb40 No-Clean Leaded Solder Wire, 0.032" (0.81 mm), 18 g (0.6 oz) Pocket Pack
  • Load image into Gallery viewer, MG Chemicals 4870-18G Sn60/Pb40 No-Clean Leaded Solder Wire, 0.032" (0.81 mm), 18 g (0.6 oz) Pocket Pack

MG Chemicals 4870-18G Sn60/Pb40 No-Clean Leaded Solder Wire, 0.032" (0.81 mm), 18 g (0.6 oz) Pocket Pack

06074870-18G
Regular price
$6.19
Sale price
$6.19
Regular price
Sold out
Unit price
per 
Shipping calculated at checkout.

MG Chemicals 4870-18G is an 18 g (0.6 oz) pocket pack of Sn60/Pb40 no-clean leaded solder wire, 0.032" (0.81 mm) in diameter. It pairs the classic 60/40 tin-lead alloy with a synthetic, spatter-resistant no-clean resin flux core. 60/40 melts a little higher and over a wider range than 63/37 solder.

Key Features

  • Sn60/Pb40 electronics-grade alloy
  • No-clean, halogen-free resin flux core
  • 0.032" (0.81 mm) diameter
  • Alloy exceeds J-STD-006C and meets ASTM B 32; flux meets J-STD-004B
  • Compact 18 g pocket pack

Specifications

Brand / model MG Chemicals 4870-18G
Alloy Sn60/Pb40 (leaded)
Diameter 0.032" (0.81 mm)
Flux type No-clean
Weight 18 g (0.6 oz)
Form Pocket pack
SKU 06074870-18G

What's Included

  • 1 pocket pack of MG Chemicals 4870 solder wire, 18 g

Ideal For

Toolbox and field repairs on electronics where a small amount of leaded solder is enough.

Frequently Asked Questions

60/40 vs 63/37 solder?
63/37 melts at a single temperature (eutectic), while 60/40 goes through a short pasty range as it cools. Both are standard leaded electronics solders.

Do I need to clean the board afterward?
The flux is no-clean, so residue is normally left in place.

Contains lead (Sn60/Pb40 alloy).